Dry the TPU before producing coated webbing

Generally, raw TPU should be dry for two to three hours before processing. Why?


Raw TPU will be a little bit wet after long placing. If it is not dried, the wet raw TPU will have bad impact on the next process. The most obvious effect is which on final products. For example, it can result into the bubble or some lines on TPU webbing. In addition, the property of TPU will decline to only 70%. But aftea Generally, raw TPU is supposed to dry in temperature of 95℃ to 100%℃ for two hours.

 

manufacturing shop



Links:    FacebookTwitterPinterestYoutube

Contact Us

Adress: Junli Park, Wanjiang District, Dongguan,Guangdong,China

Zip: 523000

Mobile / WhatsApp:+86-13809829636

Tel: +86-769-23152906

Fax: +86-769-23182640

Email: sales@sunmolin.com

* Your Name:

* Your whatsapp:

* Your E-mail:

* Your-Message:

© Copyright   Sunmolin Plastic Co.,Ltd    ICP No.: 粤ICP备14090689号-5     Powered by www.gdwl.net.cn   

* Please leave your information and message in the form. We'll reply you via email as soon as possible.